Iron oxide with 90% and 70% purities was extracted from Malaysian ilmenite as shown in Fig. 2. Ilmenite cracking was performed by mixing ilmenite mineral with NaOH beads and fusing the mixture in a furnace at 550 °C for 3 h. After the washing and filtration process, the solid sample underwent acid leaching.